Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8 g/cm³ Show Supplier Material materials with Dichte of 8 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.15 - 0.6 % Show Supplier Material materials with Aluminium of 0.15 - 0.6 % | |
Chrom | 19 - 23 % Show Supplier Material materials with Chrom of 19 - 23 % | |
Eisen | 39.5 % Show Supplier Material materials with Eisen of 39.5 % | min. |
Kohlenstoff | 0.06 - 0.1 % Show Supplier Material materials with Kohlenstoff of 0.06 - 0.1 % | |
Kupfer | 0.75 % Show Supplier Material materials with Kupfer of 0.75 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Nickel | 30 - 35 % Show Supplier Material materials with Nickel of 30 - 35 % | |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |
Titan | 0.15 - 0.6 % Show Supplier Material materials with Titan of 0.15 - 0.6 % |