Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.2 g/cm³ Show Supplier Material materials with Dichte of 8.2 g/cm³ |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.2 % Show Supplier Material materials with Aluminium of 0.2 % | max. | |
Chrom | 19.5 - 23.5 % Show Supplier Material materials with Chrom of 19.5 - 23.5 % | ||
Eisen | balance | ||
Kobalt | 1 % Show Supplier Material materials with Kobalt of 1 % | max. | |
Kohlenstoff | 0.025 % Show Supplier Material materials with Kohlenstoff of 0.025 % | max. | |
Kupfer | 1.5 - 3 % Show Supplier Material materials with Kupfer of 1.5 - 3 % | ||
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | max. | |
Molybdän | 2.5 - 3.5 % Show Supplier Material materials with Molybdän of 2.5 - 3.5 % | ||
Nickel | 38 - 46 % Show Supplier Material materials with Nickel of 38 - 46 % | ||
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | max. | |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. | |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % | max. | |
Titan | 0.6 - 1.2 % Show Supplier Material materials with Titan of 0.6 - 1.2 % |