Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.1 g/cm³ Show Supplier Material materials with Dichte of 8.1 g/cm³ |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Eisen | balance | ||
Kohlenstoff | 0.05 % Show Supplier Material materials with Kohlenstoff of 0.05 % | max. | |
Mangan | 0.5 % Show Supplier Material materials with Mangan of 0.5 % | max. | |
Nickel | 35 - 37 % Show Supplier Material materials with Nickel of 35 - 37 % | ||
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % | max. |