Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 135 MPa Show Supplier Material materials with Biegefestigkeit of 135 MPa | ISO178 |
Biegemodul | 23.0 °C | 3.5 GPa Show Supplier Material materials with Biegemodul of 3.5 GPa | ISO178 |
Dehnung | 23.0 °C | 7.5 % Show Supplier Material materials with Dehnung of 7.5 % | ISO527 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 8 kJ/m² | ISO179 |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 70 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 70 kJ/m² | ISO179 |
Zugfestigkeit | 23.0 °C | 95 MPa Show Supplier Material materials with Zugfestigkeit of 95 MPa | ISO527 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C | ISO 75/A | |
Schmelzpunkt | 215 - 225 °C Show Supplier Material materials with Schmelzpunkt of 215 - 225 °C | ISO3146 | |
Entflammbarkeit | HB UL94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | GB/T 1408 |
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | GB/T1410 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive industry, mechanical shields, blades, gears, power tools, etc. | |
Fillers | 10% Glass Fiber |