Property | Value |
---|---|
Dichte | 3.01 g/cm³ Show Supplier Material materials with Dichte of 3.01 g/cm³ |
Mechanisch
Thermisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Glasübergangstemperatur | 430 °C Show Supplier Material materials with Glasübergangstemperatur of 430 °C | ISO 7884-8 | ||
Glühtemperatur | 435.0 °C Show Supplier Material materials with Glühtemperatur of 435.0 °C | ISO 7884-4 | Viscosity 10¹³ dPa·s | |
Koeffizient der thermischen Ausdehnung | 9.1e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9.1e-06 1/K | ISO 7991 | mean value for 20-300 °C | |
Softening temperature | 630.0 °C Show Supplier Material materials with Softening temperature of 630.0 °C | ISO 7884-3 | Viscosity 10⁷·⁶ dPa·s | |
Specific electrical resistance temperature | 330.0 °C Show Supplier Material materials with Specific electrical resistance temperature of 330.0 °C | For ρ=10⁸ Ω·cm | ||
Working temperature | 982.0 °C Show Supplier Material materials with Working temperature of 982.0 °C | ISO 7884-2 | Viscosity 10⁴ dPa·s | |
Wärmeleitfähigkeit | 90 °C | 0.9 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.9 W/(m·K) |
Elektrisch
Property | Temperature | Value | Frequency |
---|---|---|---|
Dielektrizitätskonstante | 6.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 6.6 [-] | 1MHz | |
Verlustfaktor | 0.0011 [-] Show Supplier Material materials with Verlustfaktor of 0.0011 [-] | 1MHz | |
spezifischer Widerstand | 250 °C | 3.98e+07 Ω·m Show Supplier Material materials with spezifischer Widerstand of 3.98e+07 Ω·m | |
350 °C | 398107 Ω·m Show Supplier Material materials with spezifischer Widerstand of 398107 Ω·m |
Optisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Brechungsindex | 1.6 [-] Show Supplier Material materials with Brechungsindex of 1.6 [-] | at λ=587.6 nm | |
Stress optical coefficient | 3.1e-06 mm²/N Show Supplier Material materials with Stress optical coefficient of 3.1e-06 mm²/N | DIN 52314 |
Technological properties
Property | ||
---|---|---|
Application areas | General electrotechnical application and electrotechnology (Signal intensifier, Detector and (fibre-) optics), Endoscopy. | |
Corrosion properties | Hydrolytic resistance Class HGB3 (ISO 719) - Acid resistance Class S2 (DIN 12116) - Alkali resistance Class A3 (ISO695) |