Allgemein
Property | Value |
---|---|
Dichte | 2.27 g/cm³ Show Supplier Material materials with Dichte of 2.27 g/cm³ |
Thermisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Glasübergangstemperatur | 465 °C Show Supplier Material materials with Glasübergangstemperatur of 465 °C | ISO 7884-8 | |
Glühtemperatur | 480.0 °C Show Supplier Material materials with Glühtemperatur of 480.0 °C | ISO 7884-4 | Viscosity 10¹³ dPa·s |
Koeffizient der thermischen Ausdehnung | 4.7e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4.7e-06 1/K | ISO 7991 | mean value for 20-300 °C |
Softening temperature | 715.0 °C Show Supplier Material materials with Softening temperature of 715.0 °C | ISO 7884-3 | Viscosity 10⁷·⁶ dPa·s |
Working temperature | 1130.0 °C Show Supplier Material materials with Working temperature of 1130.0 °C | ISO 7884-2 | Viscosity 10⁴ dPa·s |
Optisch
Property | Value | Comment |
---|---|---|
Brechungsindex | 1.5 [-] Show Supplier Material materials with Brechungsindex of 1.5 [-] | at λ=587.6 nm |
Chemical properties
Property | ||
---|---|---|
Other | 0.01 % | max., Lead, Cadmium, Mercury and Hexavalent Chromium |
Technological properties
Property | ||
---|---|---|
Application areas | For use in clad tube for optical fibers, Endoscopy | |
Corrosion properties | Hydrolytic resistance Class HGB2 (ISO 719) - Acid resistance Class S4 (DIN 12116) - Alkali resistance Class A3 (ISO695) |