Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 4.56 g/cm³ Show Supplier Material materials with Dichte of 4.56 g/cm³ |
Partikelgröße D50 | 0.8 - 0.9 μm Show Supplier Material materials with Partikelgröße D50 of 0.8 - 0.9 μm |
Chemical properties
Property | Value | Comment |
---|---|---|
Eisen | 0.1 % Show Supplier Material materials with Eisen of 0.1 % | Fe₂O₃ |
Titan | 0.15 % Show Supplier Material materials with Titan of 0.15 % | TiO₂ |
Zirkonium | 64.5 - 65.5 % Show Supplier Material materials with Zirkonium of 64.5 - 65.5 % | ZrO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | Plastic industry,Refractory materials,as emulsifying agent used in various types of ceramic glaze,coffee cups for export,sanitary ceramics,floor tiles,building tiles.It also can be used in making ceramics rollers and brake discs. Used for epoxy resin formulations,the sealing resin,silicones,vinyl resins,and as the filler material of resin in order to increase the heat resistance and improve the insulation value and it also used in filler materials that requires inert, fine, white and chemical resistant. Casted refractories for glass melting furnaces, heat resistant porcelain, sand flushing in refractory casting and the refractory slabs, special fire resistant porcelain, refractory cement. |