Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 69 MPa Show Supplier Material materials with Biegefestigkeit of 69 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 1.58 GPa Show Supplier Material materials with Biegemodul of 1.58 GPa | ASTM D790 |
Dehnung | 23.0 °C | 18 % Show Supplier Material materials with Dehnung of 18 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 30 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 30 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 38 MPa Show Supplier Material materials with Zugfestigkeit of 38 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 122 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 122 °C | ASTM D648 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+6 - 1.00E+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+6 - 1.00E+10 Ω/sq | ASTM D257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 12 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 12 g/10min | ASTM D1238, 230°C/5kg | |
Schrumpfung | 23.0 °C | 0.99 % Show Supplier Material materials with Schrumpfung of 0.99 % | ASTM D955, Mold Shrinkage |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS | |
Color | Black | |
Processing methods | Injection molding - Drying time: 4hrs, temperature: 120°C - Mold temperature: 100°-120°C - Injection temperature: 260°-300°C |