Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.3 - 1.34 g/cm³ Show Supplier Material materials with Dichte of 1.3 - 1.34 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Härte, Shore A | 23.0 °C | 82 - 88 [-] Show Supplier Material materials with Härte, Shore A of 82 - 88 [-] | ASTM D2240 |
Zugfestigkeit | 23.0 °C | 8 MPa Show Supplier Material materials with Zugfestigkeit of 8 MPa | ASTM D412 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1000 - 100000 Ω/sq Show Supplier Material materials with Surface resistivity of 1000 - 100000 Ω/sq | ASTM D257 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 2.2 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 2.2 g/10min | ASTM D2240, 180°C/5kg |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS | |
Color | Black | |
Processing methods | Injection molding - Drying time: 3-4hrs, temperature: 70°C - Extrusion temperature: 150-190°C |