Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.26 g/cm³ Show Supplier Material materials with Dichte of 8.26 g/cm³ | |
Porosität | 0.5 % Show Supplier Material materials with Porosität of 0.5 % | max., <10μ (pore area) |
Abmessung
Property | Value |
---|---|
Dimensions | According to the AM process requirements of our customers, VDM® Powder 718 is available in a wide range of particle fractions from 10 to 250 μm. Standard particle fractions: 10-53µm, 53-150µm |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 1270 - 1340 °C Show Supplier Material materials with Schmelzpunkt of 1270 - 1340 °C |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.4 - 0.6 % Show Supplier Material materials with Aluminium of 0.4 - 0.6 % | ||
Bismut | 5E-5 % Show Supplier Material materials with Bismut of 5E-5 % | max. | |
Blei | 1E-3 % Show Supplier Material materials with Blei of 1E-3 % | max. | |
Bor | 6E-3 % Show Supplier Material materials with Bor of 6E-3 % | max. | |
Chrom | 17 - 21 % Show Supplier Material materials with Chrom of 17 - 21 % | ||
Eisen | Balance | ||
Kobalt | 1 % Show Supplier Material materials with Kobalt of 1 % | max. | |
Kohlenstoff | 0.045 % Show Supplier Material materials with Kohlenstoff of 0.045 % | max. | |
Kupfer | 0.23 % Show Supplier Material materials with Kupfer of 0.23 % | max. | |
Mangan | 0.35 % Show Supplier Material materials with Mangan of 0.35 % | max. | |
Molybdän | 2.8 - 3.3 % Show Supplier Material materials with Molybdän of 2.8 - 3.3 % | ||
Nickel | 50 - 55 % Show Supplier Material materials with Nickel of 50 - 55 % | ||
Niobium | 4.87 - 5.2 % Show Supplier Material materials with Niobium of 4.87 - 5.2 % | Nb+Ta | |
Phosphor | 0.01 % Show Supplier Material materials with Phosphor of 0.01 % | max. | |
Sauerstoff | 0.03 % Show Supplier Material materials with Sauerstoff of 0.03 % | max. | |
Schwefel | 0.01 % Show Supplier Material materials with Schwefel of 0.01 % | max. | |
Selen | 5E-4 % Show Supplier Material materials with Selen of 5E-4 % | max. | |
Silizium | 0.35 % Show Supplier Material materials with Silizium of 0.35 % | max. | |
Tantal | 4.87 - 5.2 % Show Supplier Material materials with Tantal of 4.87 - 5.2 % | Nb+Ta | |
Titan | 0.8 - 1.15 % Show Supplier Material materials with Titan of 0.8 - 1.15 % |
Technological properties
Property | ||
---|---|---|
Application areas | Due to its excellent corrosion resistance and its good workability, VDM® Powder 718 CTP is versatile in use in the oil and gas industry, in the offshore industry and in marine engineering. The conventionally manufactured VDM® Alloy 718 CTP has proven itself well, especially for oilfield completion equipment in very demanding environments containing H₂S, CO₂, and high chlorides. The alloy has also proven itself for highly stressed oilfield components. | |
Corrosion properties | As a result of the high chromium and molybdenum concentrations, conventionally manufactured VDM® Alloy 718 CTP has very good general corrosion resistance and pitting corrosion resistance in many environments. By virtue of its high nickel content, it also has good resistance against stress corrosion. | |
Other | VDM® Powder 718 CTP has an austenitic microstructure with multiple phases. By means of different heat treatments, graduated mechanical properties of the material can be achieved. The excellent mechanical properties of VDM® Powder 718 CTP result from the γ‘‘-formation during the precipitation hardening. |