Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.03 g/cm³ Show Supplier Material materials with Dichte of 1.03 g/cm³ | ASTM D792 |
Wasserabsorption | 23.0 °C | 1.7 % Show Supplier Material materials with Wasserabsorption of 1.7 % | @24 hours | ASTM D570 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 55 MPa Show Supplier Material materials with Biegefestigkeit of 55 MPa | ASTM D790 | ||
Biegemodul | 23.0 °C | 1.8 GPa Show Supplier Material materials with Biegemodul of 1.8 GPa | ASTM D790 | ||
Dehnung | 23.0 °C | 13 % Show Supplier Material materials with Dehnung of 13 % | ASTM D638 | ||
Hardness, Rockwell R | 23.0 °C | 105 [-] Show Supplier Material materials with Hardness, Rockwell R of 105 [-] | ASTM D785 | ||
Härte, Shore D | 23.0 °C | 68 [-] Show Supplier Material materials with Härte, Shore D of 68 [-] | ASTM D2240 | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 320 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 320 J/m | ASTM D256 | ||
Streckgrenze | 23.0 °C | 34 MPa Show Supplier Material materials with Streckgrenze of 34 MPa | ASTM D638 | ||
Impact strength, Izod unnotched, ASTM | No Break, ASTM D256 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 88 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 88 °C | ASTM D648 | |
Heat deflection temperature, 1.80 MPa | 71 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 71 °C | ASTM D648 | |
Entflammbarkeit | UL94: BH |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+9 - 1.00E+11 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+9 - 1.00E+11 Ω/sq | ASTM D257 |
Volume resistivity | 23.0 °C | 1.00E+9 - 1.00E+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+9 - 1.00E+11 Ω·cm | ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas |