Acerinox is one of the most competitive companies in the world in the manufacturing of stainless steels and nickel alloys.
Hauptsitz
Madrid, Spain
Webseite
Art
Hersteller und Verarbeiter
Certifications
ISO 9001
, ISO 50001
, ISO 14001
Grade | Shape | ||
---|---|---|---|
EN 1.4016 | Billet | EN 1.4016, EN X6Cr17, AISI 430 | EN 10088 |
EN 1.4031 | Disc | EN 1.4031, EN X39Cr13, AISI 420 | EN 10088 |
EN 1.4104 | Bar | EN 1.4104, EN X14CrMoS17 | |
EN 1.4105 | Billet | EN 1.4105, EN X6CrMoS17, AISI 430F | EN 10088 |
EN 1.4113 | Billet | EN 1.4113, EN X6CrMo17-1, AISI 434 | EN 10088 |
EN 1.4116 | Disc | EN 1.4116, EN X50CrMoV15, AISI 420MoV | EN 10088 |
EN 1.4301 | Billet | EN 1.4301, EN X5CrNi18-10, AISI 304 | EN 10088 |
EN 1.4303 | Billet | EN 1.4303, EN X4CrNi18-12, AISI 305 | EN 10088 |
EN 1.4305 | Billet | EN 1.4305, EN X8CrNiS18-9, AISI 303 | EN 10088 |
EN 1.4306 | Billet | EN 1.4306, EN X2CrNi19-11, AISI 304L | EN 10088 |