Allied Copper Alloys are processors, stockists and distributors of Brass, Copper, Phosphor Bronze, Nickel Silver and Stainless Steel Precision Rolled Strip and Wire.
Hauptsitz
Birmingham, United Kingdom
Art
Processor and Distributor
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
BS 301S21 | Coil | BS 301S21 | BS 1449 |
BS 304S11 | Coil | BS 304S11 | BS 1449 |
BS 304S15 | Coil | BS 304S15 | BS 1449 |
BS 304S31 | Coil | BS 304S31 | BS 1449 |
BS 316S11 | Coil | BS 316S11, EN 1.4404 | BS 1449 |
BS 409S19 | Coil | BS 409S19 | BS 1449 |
BS 420S45 | Coil | BS 420S45 | BS 1449 |
BS 430S17 | Coil | BS 430S17 | BS 1449 |
DIN 1.4310 | Coil | DIN 1.4310 | EN 10088 |
EN 1.4016 | Coil | EN 1.4016 | EN 10088 |