First begin with Yao Teng Steel Brand, Otai Steel supplies a wide range of carbon, alloy and stainless steel products, including high speed tool steel, cold works tool steel, hot works tools steel, plastic mould steel, engineering steel and machine structural steel etc.
Hauptsitz
Dongguan,Guangdong, China
Webseite
Art
Hersteller und Verarbeiter
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
AISI A2 | Bar, Plate, Slab | AISI A2, UNS T30102, DIN 1.2363, DIN X100CrMoV5, JIS SKD12, BS BA2 | ASTM A681, DIN EN ISO 4957, JIS G4404, BS 4659 |
AISI D2 | Bar, Plate, Slab | AISI D2, DIN 1.2379, DIN X153CrMo12, JIS SKD11 | ASTM A681, DIN EN ISO 4957, JIS G4404 |
AISI D6 | Bar, Plate | AISI D6, DIN 1.2436, JIS SKD2 | ASTM A681, DIN EN ISO 4957, JIS G4404 |
AISI H13 | Bar, Plate, Slab | AISI H13, DIN 1.2344, DIN X40CrMoV5-1, JIS SKD61 | ASTM A681, DIN EN ISO 4957, JIS G4404 |
ASTM 1045 | Bar, Plate | ASTM 1045, DIN 1.1191, DIN C45, JIS S45C, AS 1045 | ASTM A29, EN 100832, JIS G4051, AS 1442 |
ASTM 4340 | Bar, Plate | ASTM 4340, EN 36CrNiMo4, DIN 1.6511, BS EN24, BS 817M40, JIS SNCM439, JIS SNCM8 | ASTM A29, EN 10250, BS 970, JIS G4103 |
ASTM 5140 | Bar, Plate, Block | ASTM 5140, EN 41Cr4, JIS SCr440 | ASTM A29, EN 100833, JIS G4053 |
ASTM 8620 | Bar | ASTM 8620, DIN 1.6523, DIN 21NiCrMo2, EN 20NiCrMo2-2, BS 805M20, JIS SNCM220 | ASTM A29, DIN 1654-2, EN 10084, BS 970, JIS G4103 |
ASTM A420 Grade WPL6 | Plate | ASTM A420 Grade WPL6 | ASTM A681, DIN EN ISO 4957, GB/T 1299 |
ASTM D3 | Bar, Plate, Slab | ASTM D3, DIN 1.2080, DIN X210Cr12, JIS SKD1 | ASTM A681, DIN EN ISO 4957, JIS G4404 |