As the team behind Australasia’s largest supplier of stainless and specialty steel products, the people of Atlas Steels are driven by wanting to be our customers’ first choice in specialty metals.
Hauptsitz
Ingleburn,New South Wales, Australia
Webseite
Art
Hersteller und Verarbeiter
Grade | Shape | ||
---|---|---|---|
AISI 301 | Bar | AISI 301, UNS S30100, EN 1.4319, EN X5CrNi17-7, JIS SUS301 | ASTM A666, EN 10088-2, JIS G4305 |
AISI 301L | Bar | AISI 301L, UNS S30103, JIS SUS301L | ASTM A666, EN 10088-2, JIS G4305 |
AISI 301LN | Bar | AISI 301LN, UNS S30153, EN 1.4318, EN X2CrNiN18-7 | ASTM A666, EN 10088-2, JIS G4305 |
AISI 302HQ | Bar | AISI 302HQ, UNS S30430, EN 1.4567, EN X3CrNiCu18-9-4, JIS SUSXM7 | ASTM A493 |
AISI 303 | Bar | AISI 303, UNS S30300, EN 1.4305, EN X8CrNiS18-9, SS 2346, JIS SUS303 | ASTM A582 |
AISI 303Se | Bar | AISI 303Se, UNS S30323, JIS SUS303Se | ASTM A582 |
AISI 304 | Sheet, Coil, Strip, Plate, Tube, Pipe, Bar | AISI 304, UNS S30400, EN 1.4301, EN X5CrNi18-10, SS 2332, JIS SUS304 | ASTM A240 |
AISI 304H | Sheet, Coil, Plate | AISI 304H, UNS S30409, EN 1.4948, EN X6CrNi18-11 | ASTM A240 |
AISI 304L | Sheet, Coil, Strip, Plate, Tube, Pipe, Bar | AISI 304L, UNS S30403, EN 1.4307, EN X2CrNi18-9, SS 2352, JIS SUS304L | ASTM A240 |
AISI 310 | Sheet, Coil, Plate | AISI 310, UNS S31000 | ASTM A167 |