Aubert & Duval has contributed to the projects of the most demanding industries. Today, Aubert & Duval, a specialist in upscale metallurgy, is a world leader in designing, developing and industrialising high-performance steel, superalloy, aluminum or titanium parts.
Hauptsitz
Paris, France
Webseite
Art
Hersteller und Verarbeiter
Certifications
ISO 14001
, ISO 50001
Grade | Shape | ||
---|---|---|---|
CoCr20W15Ni | Bar | CoCr20W15Ni, UNS R30605 | |
CoCr28Mo | Bar | CoCr28Mo, UNS R31537 | |
DIN AlCu35LiAgMg | Bar | DIN AlCu35LiAgMg, UNS A92050, AA 2050, EN AW-2050 | |
DIN AlCu4Mg1 | Bar | DIN AlCu4Mg1, UNS A92024, ISO AlCu4Mg1, AA 2024, EN AW-2024 | |
DIN AlCu6Mn | Bar | DIN AlCu6Mn, UNS A92219, ISO AlCu6Mn, AA 2219, EN AW-2219 | |
DIN AlMg4.5Mn0.7 | Bar | DIN AlMg4.5Mn0.7, UNS A95083, ISO AlMg4.5Mn0.7, AA 5083, EN AW-5083 | |
DIN AlZn4.5Mg1 | Bar | DIN AlZn4.5Mg1, UNS A97020, ISO AlZn4.5Mg1, AA 7020, EN AW-7020 | |
DIN AlZn5.5MgCu(B) | Bar | DIN AlZn5.5MgCu(B), UNS A97175, AA 7175, EN AW-7175 | |
DIN AlZn6CuMgZr | Bar | DIN AlZn6CuMgZr, UNS A97050, ISO AlZn6CuMgZr, AA 7050, EN AW-7050 | |
DIN AlZn6MgCu | Bar | DIN AlZn6MgCu, UNS A97010, ISO AlZn6MgCu, AA 7010, EN AW-7010 | |