Manufacturer of specification Aluminium & Copper alloy ingots and a physical processor and trader of scrap Aluminium, Copper, Nickel and Cobalt revert alloys and an extensive range of exotic minor metals including Chromium, conflict-free Tantalum, Niobium, Molybdenum, Tungsten, Rhenium, Hafnium, Zirconium, Vanadium, Manganese, Silicon and Magnesium.
Hauptsitz
Gloucester, United Kingdom
Webseite
Art
Hersteller und Verarbeiter
Certifications
ISO 9001
, ISO 14001
, ISO 50001
Grade | Shape | ||
---|---|---|---|
AFNOR A-S2GT | Ingot | AFNOR A-S2GT, EN AB-41000, EN AB-AlSi2MgTi | |
EN AB-21000 | Ingot | EN AB-21000, EN AB-AlCu4MgTi | |
EN AB-21100 | Ingot | EN AB-21100, EN AB-AlCu4Ti | |
EN AB-42000 | Ingot | EN AB-42000, EN AB-AlSi7Mg | |
EN AB-42100 | Ingot | EN AB-42100, EN AB-AlSi7Mg0.3 | |
EN AB-42200 | Ingot | EN AB-42200, EN AB-AlSi7Mg0.6 | |
EN AB-43000 | Ingot | EN AB-43000, EN AB-AlSi10Mg(A) | |
EN AB-43100 | Ingot | EN AB-43100, EN AB-AlSi10Mg(B) | |
EN AB-43200 | Ingot | EN AB-43200, EN AB-AlSi10Mg(Cu) | |
EN AB-43300 | Ingot | EN AB-43300, EN AB-AlSi9Mg | |