BE Group is a trading and service company, offering a broad range of steel, stainless steel and aluminium products. With extensive expertise and efficient processes in purchasing, logistics and production, we offer inventory sales, production service and direct deliveries to customers based on their specific needs for steel and metal products.
Hauptsitz
Malmö, Sweden
Webseite
Art
Vertreiber
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
AR450 | Beam, Bar, Profile, Sheet, Pipe, Section | AR450 | EN 10025-2, EN 10028 |
EN 1.4301 | Plate, Bar, Angle, Profile, Tube, Pipe | EN 1.4301 | ISO 9445, EN 10088-2, EN 10028-7, EN 10204-3.1, EN ISO 9444, ISO 18286, EN 10088-3, EN 10059, EN 10056-2, EN 10279, EN 10219-2 |
EN 1.4305 | Bar | EN 1.4305 | EN 10060, EN 10088-3, EN 10204-3.1, EN 10278 |
EN 1.4307 | Bar, Pipe, Tube | EN 1.4307 | EN 10088-2, EN 10028-7, EN 10204-3.1, EN 10058, EN ISO 1127, EN 10217-7 |
EN 1.4362 | Bar | EN 1.4362 | EN 10204-3.1 |
EN 1.4404 | Bar, Plate, Angle | EN 1.4404 | ISO 9445, EN 10088-2, EN 10028-7, EN 10204-3.1, EN ISO 9444, ISO 18286, EN 10088-3, EN 10060, EN 10278, EN 10059, EN 10056-2 |
EN 1.4460 | Bar | EN 1.4460 | EN 10060, EN 10088-3, EN 10204-3.1 |
EN 1.4462 | Plate | EN 1.4462 | EN 10088-2, EN 10028-7, ISO 18286, EN 10088-3 |
EN 1.4571 | Tube, Pipe | EN 1.4571 | EN 10219-2, EN 10088-2, EN 10204-3.1 |
EN 1.4835 | Plate | EN 1.4835, Alloy 253MA | ISO 9445, EN 10088-2, EN 10028-7, EN 10204-3.1 |