Having three cold-rolling and three hot dip galvanized steel lines, Borçelik is the biggest galvanized steel manufacturer of Turkey offering the highest quality with 900 thousand tons of galvanized steel capacity.
Hauptsitz
BURSA, Turkey
Webseite
Art
Hersteller und Verarbeiter
Certifications
IATF 16949
, ISO 9001
, ISO 50001
Grade | Shape | ||
---|---|---|---|
DP450 | Coil, Sheet | DP450 | |
DP500 | Coil, Sheet | DP500 | |
DP600 | Coil, Sheet | DP600 | |
DP800 | Coil, Sheet | DP800 | |
EN 51CrV4 | Coil, Sheet | EN 51CrV4 | |
EN C40 | Coil, Sheet | EN C40 | |
EN C45 | Coil, Sheet | EN C45 | |
EN C50 | Coil, Sheet | EN C50 | |
EN C55 | Coil, Sheet | EN C55 | |
EN C60 | Coil, Sheet | EN C60 | |