Grade | Shape | ||
---|---|---|---|
BS 815M17 | Bar | BS 815M17 | EN 10277, BS 970, EN 10084 |
EN 10S20 | Bar | EN 10S20 | EN 10277, EN 10087 |
EN 10SPb20 | Bar | EN 10SPb20 | EN 10277, EN 10087 |
EN 11SMn30 | Bar | EN 11SMn30, BS 230M07, ASTM 1215 | EN 10277, BS 970, ASTM A29, EN 10087 |
EN 11SMn37 | Bar | EN 11SMn37, BS 240M07 | EN 10277, BS 970, EN 10087 |
EN 11SMnPb30 | Bar | EN 11SMnPb30, BS 230M07, ASTM 12L14 | EN 10277, BS 970, ASTM A29, EN 10087 |
EN 11SMnPb37 | Bar | EN 11SMnPb37, BS 240M07 | EN 10277, BS 970, EN 10087 |
EN 15Mn13 | Bar | EN 15Mn13, BS 210M15, ASTM 1117 | EN 10277, BS 970, ASTM A29, EN 10087 |
EN 15NiCr13 | Bar | EN 15NiCr13, BS 655M13 | EN 10277, BS 970, EN 10084 |
EN 16MnCrB5 | Bar | EN 16MnCrB5 | EN 10277, EN 10084 |