Cogne Acciai Speciali is a steel company based in Aosta Valley, leader in stainless steel long products.Its mission is specializing in niche markets and responding professionally to all the needs of its customers.
Hauptsitz
Aosta (AO), Italy
Webseite
Art
Hersteller und Verarbeiter
Certifications
ISO 14001
, ISO 45001
, ISO 9001
, NORSOK M-650
, AD 2000
, IATF 16949
, ISO 9001
Grade | Shape | ||
---|---|---|---|
Cogne 329/1 | Bar, Wire, Rod | EN X3CrNiMoN27-5-2, EN 1.4460, AFNOR Z3CND25-07Az, SS 2324, JIS SUS329J1, ASTM 329, UNS S32900, UNS J93371 | |
Cogne 329A | Bar, Wire, Rod | EN X2CrNiMoN22-5-3, EN 1.4462, BS 318S13, AFNOR Z2CND24-08Az, JIS SUS329J3L, ASTM F51, UNS S31803 | |
Cogne 329S | Bar, Wire, Rod | EN X2CrNiMoCuWN25-7-4, EN 1.4501, AFNOR Z3CNDU25-06Az, ASTM F55, UNS S32760 | |
Cogne 329S1 | Bar, Wire, Rod | EN X2CrNiMoN25-7-4, EN 1.4401, AFNOR Z3CND25-06Az, SS 2328, ASTM F53, UNS S32750, Alloy 2507 | |
Cogne 347 | Bar, Wire, Rod | EN X6CrNiNb18-10, EN 1.4550, BS 347S31, AFNOR Z6CNNb18-10, SS 2338, JIS SUS347, ASTM 347, UNS S34700 | |
Cogne 350 | Bar, Wire, Rod | EN 1.3964, ASTM XM-19, UNS S20910 | |
Cogne 354 | Bar, Wire, Rod | EN X1CrNiMoCuN20-18-7, EN 1.4547, SS 2378, ASTM F44, Alloy 254SMO | |
Cogne 616C | Bar, Wire, Rod | EN X20CrMoV12-1, EN X22CrMoV12-1, EN 1.4922, EN 1.4923, BS 762, AFNOR Z21CDV12, SS 2317 | |
Cogne 630 | Bar, Wire, Rod | EN X5CrNiCuNb16-4, EN 1.4542, AFNOR Z7CNU17-04, JIS SUS630, ASTM 630, 17-4 PH, UNS S17400, UNS J92180 | |
Cogne 904L | Bar, Wire, Rod | EN X1NiCrTiMoCu25-20-5, EN 1.4539, BS 904S13, AFNOR Z2CNDU25-20-5, SS 2562, AISI 904L, UNS N08904 | |