Grade | Shape | ||
---|---|---|---|
BS 080A15 | Bar | BS 080A15 | |
BS 080A42 | Bar, Plate | BS 080A42 | |
BS 230M07 | Bar | BS 230M07, BS EN1A | BS 970 |
BS 709M40 | Bar | BS 709M40 | |
BS 817M40 | Bar | BS 817M40 | |
EN C45 | Bar | EN C45 | EN10083 |
EN DD11 | Sheet, Plate | EN DD11 | EN 10111 |
EN DX51D | Sheet | EN DX51D | EN10346 |
EN S235JR | Plate | EN S235JR | EN 10025 |
EN S235JRH | Section | EN S235JRH | EN 10219 |