We produce open die forgings from 10 kg to 35,000 kg and rings with a diameter of up to 3500 mm.
Hauptsitz
Remscheid,North Rhine-Westphalia, Germany
Webseite
Art
Hersteller und Verarbeiter
Certifications
ISO 9001
, ISO 14001
, ISO 50001
, KTA 1401
, AD 2000
Grade | Shape | ||
---|---|---|---|
EN 100Cr6 | Bar, Ring, Block, Plate | EN 100Cr6, DIN 1.3505 | ISO 683-17 |
EN 100CrMnSi6-4 | Bar, Ring, Block, Plate | EN 100CrMnSi6-4, DIN 1.3520 | ISO 683-17 |
EN 100CrMo7-3 | Bar, Ring, Block, Plate | EN 100CrMo7-3, DIN 1.3536 | ISO 683-17 |
EN 11CrMo9-10 | Bar, Ring, Block, Plate | EN 11CrMo9-10, DIN 1.7383, ASTM F22 | ASTM A182, EN 10222-2 |
EN 13CrMo4-5 | Bar, Ring, Block, Plate | EN 13CrMo4-5, DIN 1.7335, ASTM F12 | ASTM A182, EN 10222-2 |
EN 15NiCr13 | Bar, Ring, Block, Plate | EN 15NiCr13, DIN 1.5752, SAE 3310 | EN 10084 |
EN 16MnCr5 | Bar, Ring, Block, Plate | EN 16MnCr5, DIN 1.7131, SAE 5115 | EN 10084 |
EN 16Mo3 | Bar, Ring, Block, Plate | EN 16Mo3, DIN 1.5415, ASTM A204 Grade A | ASTM A204, EN 10222-2 |
EN 16NiCrMoV11-6 | Bar, Ring, Block, Plate | EN 16NiCrMoV11-6, DIN 1.6948 | |
EN 17CrNi6-6 | Bar, Ring, Block, Plate | EN 17CrNi6-6, DIN 1.5918, SAE 3215 | DIN 17210 |