At Fix Metall we sell a wide variety of metals including Hot-Rolled Steel, Cold-Rolled Steel, Stainless Steel, Alloy Steel, Galvanized Steel, Tool Steel, Aluminum, Copper, Bronze, Brass and Plastics.We provide One Stop Shopping for small Quantities of any Metal, Cut & Ready, Fast. Orders can be cut to your exact specification while you wait. It's that easy.
Hauptsitz
Brunn am Gebirge, Austria
Webseite
Art
Processor and Distributor
Grade | Shape | ||
---|---|---|---|
AISI 303 | Bar | AISI 303, EN 1.4305, EN X8CrNiS18-9 | EN 10088-3 |
AISI 316 | Bar | AISI 316, EN 1.4571 | |
DIN 2.1090 | Bar | DIN 2.1090, DIN GC-CuSn7ZnPb, EN CC493K | EN 1982 |
DIN 3.3206 | Tube | DIN 3.3206, EN AW-6060, DIN AlMgSi0.5 | DIN EN 755-2 |
DIN CuZn44Pb2 | Bar | DIN CuZn44Pb2, EN 2.0375, EN CW624N | |
EN 1.7131 | Bar | EN 1.7131, EN 16MnCrS5 | EN 10277-4 |
EN AW-1050A | Sheet | EN AW-1050A, DIN 3.0255, EN AW-Al99.5 | |
EN CuZn37 | Sheet | EN CuZn37, EN CW508L, EN 2.0321 | EN 12165, DIN 17672, DIN 1759 |
EN CW004A | Sheet | EN CW004A, ISO Cu-ETP, DIN 2.0060 | |
EN X210Cr12 | Bar | EN X210Cr12, AISI D3, EN 1.2080 | DIN EN 10060 |