The company’s products included materials that had a surface of precious metal, for the desired appearance and cosmetic characteristics, but combined with additional metals which would enhance mechanical properties and reduced precious metal content and cost. This was the start of clad metals at Engineered Materials Solutions.
Hauptsitz
Attleboro,Massachusetts, United States
Webseite
Art
Hersteller und Verarbeiter
Grade | Shape | ||
---|---|---|---|
Invar 42 | Coil | Invar 42 | |
Nickel 200 | Coil | Nickel 200 | |
Nickel 201 | Coil | Nickel 201 | |