Erasteel is a major player in the HSS market with high-end conventional and powder metallurgy high speed steels.With its ASP® range, Erasteel is one leading producer of PM HSS for high performance tooling and components.
Hauptsitz
Paris, France
Webseite
Art
Hersteller und Verarbeiter
Certifications
ISO 9001
, ISO 14001
Grade | Shape | ||
---|---|---|---|
ABC III | Strip, Sheet | EN HS3-3-2, DIN 1.3333 | |
ASP 2004 | Bar, Coil | EN HS6-5-4, DIN 1.3361 | |
ASP 2005 | Bar | EN HS3-3-4, DIN 1.3377 | |
ASP 2009 | Bar, Coil | ||
ASP 2011 | Bar, Sheet, Coil | AISI A11 | |
ASP 2012 | Bar | EN HS2-2-2, DIN 1.3397 | |
ASP 2015 | Bar | EN HS12-0-5-5, DIN 1.3202, AISI T15 | |
ASP 2023 | Bar, Sheet, Strip, Coil | EN HS6-5-3C, SS 2725, JIS SKH53, DIN 1.3395, AISI M3 | |
ASP 2030 | Bar, Sheet, Coil | EN HS6-5-3-8, SS 2726, DIN 1.3294 | |
ASP 2042 | Bar, Wire | EN HS2-9-1-8, DIN 1.3247, JIS SKH59, AISI M42 | |