In the cast product and rolled product sectors, the components produced in South Westphalia are not normally visible to the end consumer. However, these product sectors play an important economic role, since they showcase the company's expertise in materials and processes.
Hauptsitz
Olpe,North Rhine-Westphalia, Germany
Webseite
Art
Hersteller und Verarbeiter
Certifications
ISO 9001
, ISO 14001
, ISO 50001
Grade | Shape | ||
---|---|---|---|
EN CC499K | Casting | EN CC499K, EN CuSn5Zn5Pb2 | DIN 50930-6, DIN EN 1982, DIN 1988 |
EN Cu-ETP | Coil | EN Cu-ETP, EN CW004A, UNS C11000 | |
EN Cu-PHC | Coil | EN Cu-PHC, EN CW020A, UNS C10300 | |
EN CuSn10 | Coil | EN CuSn10, UNS C52400 | |
EN CuSn10-C-GS | Casting | EN CuSn10-C-GS, EN CC480K, DIN G-CuSn10, EN 2.1050 | DIN EN 1982, DIN 1705, DIN 1716 |
EN CuSn12-C-GS | Casting | EN CuSn12-C-GS, EN CC483K, DIN G-CuSn12, EN 2.1052 | DIN EN 1982, DIN 1705, DIN 1716 |
EN CuSn12Ni2-C-GS | Casting | EN CuSn12Ni2-C-GS, EN CC484K, DIN G-CuSn12Ni, EN 2.1060 | DIN EN 1982, DIN 1705, DIN 1716 |
EN CuSn3Zn8Pb5-C-GS | Casting | EN CuSn3Zn8Pb5-C-GS, EN CC490K, DIN G-CuSn2ZnPb, EN 2.1098 | DIN EN 1982, DIN 1705, DIN 1716 |
EN CuSn4 | Coil | EN CuSn4, EN CW450K, UNS C51100 | |
EN CuSn4Zn2Ps | Casting | EN CuSn4Zn2Ps | DIN 2701 |