We specialise in the production and processing of tungsten and molybdenum. Both are heavy metals with unique properties. Tungsten is the pure metal with the highest melting point and the second-highest boiling point. High density, hardness and strength are its key characteristics.
Molybdenum is a high-strength, ductile metal with the highest melting point in its period group at 3422°C. We produce materials, semi-finished and finished goods through complex processes including mixing, admixing, electric sintering & reduction, deformation & annealing processes.
Hauptsitz
Traunstein, Germany
Webseite
Umsatz
11-100M USD
Anzahl der Mitarbeiter
101-200
Gründungsjahr
1911
Art
Hersteller
Qualitätszertifikate
ISO9001-2015
Elektrotechnik
Herstellung
Drähte und Kabel
Elektroden
Komponenten für Elektrogeräte
Schweißung
Components For Rotating Machines
Rotierende Maschinen
Drähte
Oberflächenbearbeitung und -beschichtung
Elektronik
Elektronische Rohre
Schneiden
Schneidwerkzeuge
Schweißausrüstung
Thermisches Spritzen
Bearbeitung
Gießformen
Schmiedegesenk
Sonstige Werkzeugmaschinen
Spanlose Arbeitsausrüstung
Strahlungsschutz
Umwelt, Gesundheit, Sicherheit
Werkzeugmaschinensysteme
Workpiece Holding Devices
Elektrische Kontakte
Welding Processes
Commercial & Industrial Heating Appliances
Domestic
Healthcare
Heizelemente
Konsumgüter
Medizinische Ausrüstung
Metallbeschichtungen
Metallurgie
Produktion von Metallen
Radiografische Ausrüstung
Grade | Shape | ||
---|---|---|---|
Molybdenum | Rod, Plate, Block | Molybdenum | |
Pure Tungsten | Rod | Pure Tungsten | |
Triamet | Rod, Plate, Block | Triamet | |
Tungsten Cerium | Rod | WCe20 | |
Tungsten Lanthanum Oxide (WL10) | Rod | WLa10 | |
Tungsten Lanthanum Oxide (WL15) | Rod | WLa15 | |
Tungsten Lanthanum Oxide (WL20) | Rod | WLa20 | |
Tungsten Thorium (WTh10) | Rod | WTh10 | |
Tungsten Thorium (WTh20) | Rod | WTh20 | |
Tungsten Thorium (WTh30) | Rod | WTh30 | |