Customers depend on Ranger Steel to deliver what they need when and where they want it. We build business relationships that last with our quality products, competitive prices and outstanding service. That's why we have become the steel plate provider of choice.
Hauptsitz
Houston,Texas, United States
Webseite
Art
Processor and Distributor
Grade | Shape | ||
---|---|---|---|
ASME SA516 Grade 60 | Plate | ASME SA516 Grade 60 | ASME SA516 |
ASME SA516 Grade 70 | Plate | ASME SA516 Grade 70 | ASME SA516 |
ASTM A36 | Plate | ASTM A36 | ASTM A36 |
ASTM A572 Grade 50 | Plate | ASTM A572 Grade 50 | ASTM A572 |
ASTM A572 Grade 65 | Plate | ASTM A572 Grade 65 | ASTM A572 |
ASTM A588 Grade A | Plate | ASTM A588 Grade A | ASTM A588 |
ASTM A588 Grade B | Plate | ASTM A588 Grade B | ASTM A588 |
ASTM A709 Grade 50 Type 1 | Plate | ASTM A709 Grade 50 Type 1, ASTM A709 Grade 50 Type 2, ASTM A709 Grade 50 Type 3 | ASTM A709 |
ASTM A871 Grade 65 | Plate | ASTM A871 Grade 65 | ASTM A871 |