Grade | Shape | ||
---|---|---|---|
17-4 PH | Bar | 17-4 PH | |
BS 070M20 | Bar | BS 070M20, BS 080A15, DIN 1.0401, EN 1.0401, DIN 1.0402, DIN 1.0511, EN 1.0511, AISI 1020, SAE 1020, ASTM 1023, DIN C15, BS EN3A | |
BS 070M55 | Bar | BS 070M55, BS EN9, EN 1.0535, DIN 1.0535, AISI 1055, SAE 1055, DIN C55 | BS 970 |
BS 080A42 | Bar | BS 080A42 | |
BS 080M40 | Bar | BS 080M40, BS EN8, AISI 1040, SAE 1040, DIN C40 | BS 970 |
BS 080M46 | Bar | BS 080M46 | |
BS 080M50 | Bar | BS 080M50 | |
BS 230M07 | Bar | BS 230M07 | |
BS 535A99 | Bar | BS 535A99, BS EN31, EN 1.3505, DIN 1.3505, AISI 52100, SAE 52100 | BS 970 |
BS 635M15 | Bar | BS 635M15, EN 1.5714, DIN 1.5714, EN 16NiCr4, DIN 16NiCr4 | |