Munich as a representative for Italian steel and rolling mills.
Hauptsitz
Munich,Bavaria, Germany
Webseite
Art
Hersteller und Verarbeiter
Grade | Shape | ||
---|---|---|---|
EN 11SMn37 | Bar | EN 11SMn37, EN 1.0736 | EN 10087 |
EN 11SMnPb37 | Bar | EN 11SMnPb37, EN 1.0737 | EN 10087 |
EN 15B2 | Bar | EN 15B2, EN 1.5501 | EN 10263 |
EN 18B2 | Bar | EN 18B2, EN 1.5503 | EN 10263 |
EN 19MnB4 | Bar | EN 19MnB4, EN 1.5523 | EN 10263, EN 10269, EN 10083 |
EN 21CrMo4 | Bar | EN 21CrMo4, EN 1.7255 | EN 10263, EN 10269, EN 10083 |
EN 30MnB4 | Bar | EN 30MnB4, EN 1.5526 | EN 10263, EN 10269, EN 10083 |
EN 34Cr4 | Bar | EN 34Cr4, EN 1.7033 | EN 10263, EN 10269, EN 10083 |
EN 34CrMo4 | Bar | EN 34CrMo4, EN 1.7220 | EN 10263, EN 10269, EN 10083 |
EN 35B2 | Bar | EN 35B2, EN 1.5511 | EN 10263, EN 10269, EN 10083 |