We found that we could effectively take on the logistics of production, stocking, packaging and shipping. This was accomplished within a strict cost structure that allowed us to directly compete at mill price levels while outperforming traditional metals service centers on service. This would also allow us to accomplish several major objectives for our customers: Direct participation with OEMs in designing alloys to meet specific performance objectives. Eliminating large purchasing commitments by the subcontractors. Producing the exact size and shape bar to drive down machining costs. Delivering the exact quantity of material required for a particular production run on the exact day it is needed for smooth material flow. Packaging according to customer preference to ease handling at their facility. Assuming responsibility for job-specific labeling to eliminate relabeling by our customers. Commitment to managing production and shipping schedules to guarantee metal on the floor. Always having the ability to quickly expand production and warehousing in response to customer demand.
Hauptsitz
Schaumburg,Illinois, United States
Webseite
Art
Hersteller und Verarbeiter
Grade | Shape | ||
---|---|---|---|
Interbronze H7,Interbronze H7-LL | Bar | UNS C67300 | |
UNS C35300 | Profile | UNS C35300 | |
UNS C35330 | Bar, Profile | UNS C35330 | |
UNS C36000 | Profile | UNS C36000 | |
UNS C37710 | Profile | UNS C37710 | |
UNS C38500 | Profile | UNS C38500 | |
UNS C46400 | Bar | UNS C46400 | |
UNS C48200 | Bar | UNS C48200 | |
UNS C48500 | Bar | UNS C48500 | |
UNS C53400 | Bar | UNS C53400 | |