Chrome Nickel Alloys Limited a global distributor of specialised materials. Our product range covers Aluminium, Titanium, Stainless, Nickel Alloys, Maraging and Special Steels. With our comprehensive range of Rounds, Flats, Tubes, Plates, Sheets and Forging stock in the form of ingot and billet we have become a major supplier in the Aerospace, Oil and Gas, Defense and Power Generation (turbine) industries worldwide.
Hauptsitz
Corby, United Kingdom
Webseite
Art
Processor and Distributor
Certifications
AS 9120
, ISO 9001
Grade | Shape | ||
---|---|---|---|
13-8 PH | Bar, Sheet, Plate, Strip, Wire, Forging | 13-8 PH, UNS S13800, EN 1.4534 | AMS 5629, AMS 5864, ASTM A564, ASTM A693 |
17-4 PH | Bar, Sheet, Plate, Strip, Wire, Forging | 17-4 PH, UNS S17400, EN 1.4542, EN 1.4548 | AMS 5643, AMS 5622, AMS 5604, ASTM A564, ASTM A484 |
17-7 PH | Bar, Sheet, Plate, Strip, Wire, Forging | 17-7 PH, UNS S17700, EN 1.4568 | AMS 5644, AMS 5528, AMS 5529, AMS 5678, ASTM A564, MIL-S-25043 |
AA 2014A | Bar | AA 2014A, UNS A92014 | AMS 4028, AMS 4029, ASTM B247, EN 754, EN 573 |
AA 2024 | Bar, Plate, Tube | AA 2024 | EN 573, EN 754 |
AA 2124 | Plate | AA 2124, EN 3.1924 | EN 2422 |
AA 6061 | Tube | AA 6061, UNS A96061 | ASTM B210, EN 573, EN 574 |
AA 6082 | Bar | AA 6082 | EN 573, EN 755 |
AA 7050 | Plate | AA 7050, UNS A97050 | AMS B210, AMS B211 |
AA 7075 | Bar, Plate, Tube | AA 7075 | |