We are founded in 1978 and with our continuing growth are now one of East Angalia's leading stainless steel stockholders and processors.
Hauptsitz
Cambridgeshire, United Kingdom
Webseite
Art
Processor and Distributor
Grade | Shape | ||
---|---|---|---|
AISI 303 | Bar | AISI 303, EN 1.4305 | |
AISI 304 | Angle, Sheet, Plate | AISI 304, EN 1.4301 | ASTM A403 |
AISI 304L | Angle, Sheet, Bar, Plate | AISI 304L, EN 1.4307 | |
AISI 310 | Sheet, Bar, Plate, Pipe | AISI 310 | |
AISI 316 | Angle, Sheet, Plate | AISI 316, EN 1.4401 | ASTM A403 |
AISI 316L | Angle, Sheet, Bar, Plate | AISI 316L, EN 1.4404 | |
AISI 321 | Angle, Sheet, Bar, Plate | AISI 321 | ASTM A403 |
AISI 416 | Bar | AISI 416 | |
AISI 430 | Sheet | AISI 430 | |
AISI 431 | Bar | AISI 431 | |