JACQUET is a service oriented stainless and nickel alloy processing company that provide fast turnaround and delivery. JACQUET stocks 19 different grades In plate and bar as well as offer a wide range of processing capabilities to provide customers with unique and low cost solutions to their metal needs.
Hauptsitz
Barnsley, United Kingdom
Webseite
Art
Processor and Distributor
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
AISI 304 | Sheet | AISI 304, EN 1.4301, DIN X5CrNi18-10, UNS S30400, AISI 304L | EN 10029, ASTM A482 |
AISI 316L | Sheet | AISI 316L, EN 1.4404, DIN X2CrNiMo17-13-2, UNS S31603, AISI 316 | EN 10029, ASTM A483 |
Alloy 904L | Sheet | Alloy 904L, EN X1NiCrTiMoCu25-20-5, EN 1.4539, UNS N08904 | EN 10029, ASTM A489 |
EN 1.3912 | Sheet | EN 1.3912, UNS K93600, EN Ni36 | ASTM B388 |
EN 1.4000 | Sheet | EN 1.4000, UNS S41008, EN X6Cr13 | ASTM A480, EN 10029 |
EN 1.4006 | Sheet | EN 1.4006, AISI 410, UNS S41000, EN X12Cr13, ASTM 410 | ASTM A480, EN 10029 |
EN 1.4410 | Sheet | EN 1.4410, UNS S32750, EN X2CrNiMoN25-7-4 | ASTM A480, EN 10029 |
EN 1.4432 | Sheet | EN 1.4432, EN X2CrNiMo17-12-3 | ASTM A480, EN 10029 |
EN 1.4436 | Sheet | EN 1.4436, EN X3CrNiMo17-13-3 | EN 10029, ASTM A486 |
EN 1.4438 | Sheet | EN 1.4438, EN X2CrNiMo18-15-4, AISI 317L, UNS S31703 | EN 10029, ASTM A487 |