Hauptsitz
Edmonton,Alberta, Canada
Webseite
Art
Processor and Distributor
Grade | Shape | ||
---|---|---|---|
AA 6061 | Extrusion | AA 6061 | ASTM B221 |
AISI 303 | Wire, Bar | AISI 303, UNS S30300 | ASTM A581, ASTM A582 |
ASTM 4140 | Plate | ASTM 4140 | |
ASTM MT304 | Sheet, Plate, Coil, Bar | ASTM MT304, ASTM MT304L, ASTM MT304H, UNS S30400, UNS S30409, UNS S30403 | ASTM A276, ASTM A479 |
ASTM MT310 | Sheet, Plate, Coil, Bar | ASTM MT310, ASTM MT310S, UNS S30400, UNS S30409, UNS S30403 | ASTM A276, ASTM A479 |
ASTM MT316 | Sheet, Plate, Coil, Bar | ASTM MT316, ASTM MT316L, UNS S31600, UNS S31603, UNS S31653 | ASTM A276, ASTM A479 |
ASTM MT317 | Bar, Plate | ASTM MT317, UNS S31700, UNS S31703 | |
Duplex 2205 | Bar, Plate | Duplex 2205, UNS S31803, UNS S32205 | |
Nitronic 50 | Bar, Plate | Nitronic 50 | |
UNS S17400 | Bar, Plate | UNS S17400 | ASTM A564 |