Grade | Shape | ||
---|---|---|---|
EN CuNi10Fe1Mn | Tube, Bar | EN CuNi10Fe1Mn, UNS C70600, EN CW352H, BS CN102 | BS 2874, EN 12163, ASTM B121 |
EN CuNi12Zn24 | Tube, Bar | EN CuNi12Zn24, UNS C75700, EN CW403J | BS 2870, NS 104, EN 12163, ASTM B151 |
EN CuSn10 | Tube, Bar | EN CuSn10, JIS C5212 | BS 1400, IS 28, DIN 17662, DIN 17672, ISO 427, JIS M3270, ASTM B139 |
EN CuSn10P | Tube, Bar | EN CuSn10P | BS 1400, IS 28, DIN 1705, ISO 1338, ASTM B505 |
EN CuSn10Zn2 | Tube, Bar | EN CuSn10Zn2 | ASTM B505, BS 1400, IS 306 |
EN CuSn11P | Tube, Bar | EN CuSn11P | BS 1400, IS 28, DIN 1705, ISO 1338, ASTM B505, AFNOR 53707 |
EN CuSn4Pb4Zn4 | Tube, Bar | EN CuSn4Pb4Zn4, UNS C54400 | ASTM B139 |
EN CuSn5 | Tube, Bar | EN CuSn5, UNS C51000, JIS C5102 | BS 2874, IS 7811, DIN 17662, DIN 17672, ISO 427, JIS H3270, ASTM B139 |
EN CuSn5Zn5Pb5 | Tube, Bar | EN CuSn5Zn5Pb5, UNS C83600 | ASTM B505, IS 1705, DIN 1338, BS 1400, ISO 318, SAE J461, SAE J462 |
EN CuSn6 | Tube, Bar | EN CuSn6, UNS C51900, JIS C5191 | BS 2875, BS 2870, PB-103, DIN 17662, DIN 17672, ISO 427, JIS H3270, ASTM H3270 |