The most important buyers of our flat products are vehicle manufacturers and their suppliers, tube and large tube manufacturers, cold rolling mills, retailers and the construction industry. In an integrated iron and steel works, we produce hot wide strip, steel strip, strip sheet, cold thin sheet and surface-refined products with a thickness of 0.4 to 25 mm and a width of up to 2,000 mm. The production program includes drawing, deep-drawing and special deep-drawing steels, construction and fine-grain steels as well as high-strength and ultra-high-strength steels. In addition to the steels mentioned above, the delivery program of Salzgitter Flachstahl GmbH also includes other innovative products such as high-strength micro-alloyed steels and multi-phase steels e.g. B. for use in crash-relevant areas of the vehicle body high-strength martensite phase steels e.g. B. for the production of side impact beams to increase occupant protection in the passenger compartment Starting material for the production of pipes z. B. for hydroforming organic thin-film coated sheet metal with improved corrosion protection properties, especially for use in body cavities and flanges electrolytically and hot-dip galvanized sheet metal with the best surface quality, e.g. B. for automotive skin parts.
Hauptsitz
Salzgitter,Lower Saxony, Germany
Art
Hersteller und Verarbeiter
Certifications
IATF 16949
, ISO 9001
, ISO 45001
, ISO 14001
, ISO 50001
Grade | Shape | ||
---|---|---|---|
Allwesta 360 | Strip, Coil | EN S235J0W, EN 1.8958, AFNOR E24W-3 | EN 10025-5, NFA 35-502 |
Allwesta 360 F | Strip, Coil | EN S235J2W, EN 1.8961, DIN WTSt 37-3, AFNOR E24W-4 | EN 10025-5, SEW 087, NFA 35-502 |
Allwesta 510 | Strip, Coil | EN S355J0W, EN 1.8959, AFNOR E36WB3, BS WR50B, ASTM A588 Grade A, ASTM A588 Grade B, ASTM A588 Grade K, JIS SMA50AW | EN 10025-5, NFA 35-502, ASTM A242, JIS G3114, BS 4360 |
Allwesta 510 F | Strip, Coil | EN S355J2W, EN 1.8965, DIN WTSt 52-3, AFNOR E36WB4, BS WR50C, JIS SMA50CP | EN 10025-5, NFA 35-502, JIS G3114, BS 4360, SEW 087 |
Allwesta 510 F 40 | Strip, Coil | EN S355K2W, EN 1.8967 | EN 10025-5 |
Allwesta 510 FP | Strip, Coil | EN S355J0WP, EN 1.8945, AFNOR E36WA3, BS WR50A | EN 10025-5, NFA 35-502, ASTM A242 |
Allwesta 510 P | Strip, Coil | EN S355J0WP, EN 1.8945, AFNOR E36WA3, BS WR50A | EN 10025-5, NFA 35-502, BS 4360 |
ASTM A414 Grade C | Strip, Coil | ASTM A414 Grade C | BS 1501, ASTM A414 |
ASTM A516 Grade 55 | Strip, Coil | ASTM A516 Grade 55 | ASTM A516 |
ASTM A516 Grade 60 | Strip, Coil | ASTM A516 Grade 60 | BS 1501, ASTM A516 |