Shelley Steels established in 1989 supply nitiridng steels 722M24 (EN40B), 905M39 (EN41B) and alloy steel 817M40(EN24).
Hauptsitz
Barnsley, United Kingdom
Art
Processor and Distributor
Grade | Shape | ||
---|---|---|---|
BS 722M24 | Bar | BS 722M24, EN 1.8515, EN 31CrMo12, AFNOR 30CD12 | |
BS 817M40 | Bar | BS 817M40, SAE 4340, EN 1.6582 | |
BS EN41B | Bar | BS EN41B, EN 1.8509, EN 41CrAlMo7, AFNOR 40CAD6.12, EN 41Cr4 | |