Listed on the SGX Catalist in 2007, Soon Lian Holdings Limited (the “Group” or “Soon Lian”) is a specialist supplier of aluminium alloy product with an established track record of 35 years. The beginnings of the Group started with Soon Lian Hardware Pte Ltd. Founded in 1983, it occupied a 218 sq m office-cum store in Balestier. Growing steadily, it laid the basis for the establishment of the Group which is now an international supplier with operations and warehouses in Singapore, China, Malaysia and Taiwan.
Hauptsitz
Singapore, Singapore
Webseite
Art
Manufacturer, Processor and Distributor
Grade | Shape | ||
---|---|---|---|
AA 1100 | Sheet | AA 1100 | |
AA 2024 | Sheet, Rod | AA 2024 | AMS 4040, AMS QQ-A-250/5, AMS 4037, AMS QQ-A-250/4, ASTM B221, AMS QQ-A-200/3 |
AA 3105 | Plate | AA 3105 | ASTM B209 |
AA 5052 | Plate, Sheet | AA 5052 | EN 1386, ASTM B209, AMS 4016 |
AA 5083 | Plate, Sheet | AA 5083 | EN 485, EN 573, ASTM B928 |
AA 5086 | Plate, Sheet, Angle | AA 5086 | ASTM B928, ASTM B211 |
AA 5183 | Weld Wire | AA 5183 | |
AA 5356 | Weld Wire | AA 5356 | |
AA 5383 | Plate, Sheet | AA 5383 | |
AA 5754 | Plate, Sheet | AA 5754 | EN 485, EN 573, EN 1386, ASTM B209 |