Stalatube is known worldwide as the leading provider of high strength stainless steel solutions and as the manufacturer of highly developed stainless steel hollow sections, I-beams, profiles and components. We offer the widest range of square and rectangular hollow sections in the business and have significant experience in finding the right materials and the right approach in any given situation.
Hauptsitz
Lahti, Southern Finland, Finland
Webseite
Art
Hersteller und Verarbeiter
Certifications
ISO 9001
, ISO 14001
, ISO 45001
, ISO 3834-2
Grade | Shape | ||
---|---|---|---|
EN 1.4062 | Tube | EN 1.4062, EN X2CrNi22-2, Alloy 2202 | |
EN 1.4162 | Tube | EN 1.4162, UNS S32101 | |
EN 1.4301 | Tube | EN 1.4301, AISI 304 | EN 10088-2, EN 10088-4 |
EN 1.4307 | Tube | EN 1.4307, AISI 304L | EN 10088-2, EN 10088-4 |
EN 1.4318 | Tube | EN 1.4318, AISI 301LN | EN 10088-2, EN 10088-4 |
EN 1.4362 | Tube | EN 1.4362, UNS S32304, Alloy 2304, EN X2CrNi23-4 | |
EN 1.4404 | Tube | EN 1.4404, AISI 316L | EN 10088-2, EN 10088-4 |
EN 1.4420 | Tube | EN 1.4420, AISI 316 | EN 10088-2, EN 10088-4 |
EN 1.4462 | Tube | EN 1.4462, UNS S31803, EN X2CrNiMoN22-5-3 | |
EN 1.4541 | Tube | EN 1.4541, AISI 321 | EN 10088-2, EN 10088-4 |