Staystrip Group Ltd is the leading No.1 UK supplier of stainless steel strip in coil including temper rolled strip.We also have in house rolling mills, edge dressers and a oscillate winding facility.
Hauptsitz
Birmingham, United Kingdom
Webseite
Art
Hersteller und Verarbeiter
Grade | Shape | ||
---|---|---|---|
BS 301S21 | Strip | BS 301S21, EN 1.4310 | BS 1449-2, EN 10088-2 |
BS 304S11 | Strip | BS 304S11, EN 1.4307 | BS 1449-2, EN 10088-2 |
BS 304S15 | Strip | BS 304S15, EN 1.4301 | BS 1449-2, EN 10088-2 |
BS 304S16 | Strip | BS 304S16, EN 1.4301 | BS 1449-2, EN 10088-2 |
BS 304S31 | Strip | BS 304S31, EN 1.4301 | BS 1449-2, EN 10088-2 |
BS 316S11 | Strip | BS 316S11, EN 1.4404 | BS 1449-2, EN 10088-2 |
BS 316S13 | Strip | BS 316S13, EN 1.4432 | BS 1449-2, EN 10088-2 |
BS 316S31 | Strip | BS 316S31, EN 1.4401 | BS 1449-2, EN 10088-2 |
BS 316S33 | Strip | BS 316S33, EN 1.4436 | BS 1449-2, EN 10088-2 |
BS 321S31 | Strip | BS 321S31, EN 1.4541 | BS 1449-2, EN 10088-2 |