The main product portfolio consists mainly of long rolled products - rolled wire, shaped steel, special bar steel, drawn steel, rails, wide steel, seamless tubes and metallurgical semi-finished products. Other products are coke and accompanying products arising from its production, as well as artificial compacted aggregates and granulated slag.
Hauptsitz
Třinec, Czechia
Webseite
Art
Hersteller und Verarbeiter
Certifications
ISO 9001
, ISO 14001
, IATF 16949
, ISO 50001
Grade | Shape | ||
---|---|---|---|
DIN 1.7131 | Wire, Bar, Rod | DIN 1.7131, EN 16MnCr5 | |
DIN 1.7147 | Wire, Bar, Rod | DIN 1.7147, EN 20MnCr5, EN 20MnCrB5 | |
DIN QSt 52-3 | Wire, Bar, Rod | DIN QSt 52-3, DIN 1.0569 | |
DIN StE 355 | Wire, Bar, Rod | DIN StE 355, DIN 1.0566 | |
EN 100Cr6 | Wire, Bar, Rod | EN 100Cr6, DIN 1.3505 | |
EN 100CrMnSi6-4 | Wire, Bar, Rod | EN 100CrMnSi6-4, DIN 1.3520 | |
EN 100CrMo7 | Wire, Bar, Rod | EN 100CrMo7, DIN 1.3537 | |
EN 100CrMo7-3 | Wire, Bar, Rod | EN 100CrMo7-3, DIN 1.3536 | |
EN 10CrMo9-10 | Wire, Bar, Rod | EN 10CrMo9-10, DIN 1.7380 | |
EN 11SMn30 | Wire, Bar, Rod | EN 11SMn30, DIN 1.0715 | |