Ugitech is one of the world's leading manufacturers of stainless steel long products.
The company's main products are: billets, bars, wire rod and drawn wire, which the company manufactures in its own steelworks and transforms in its hot rolling mills, finishing shops and wire drawing plants.
Stainless steels are characterized by their high mechanical properties and their corrosion resistance. They are used for the manufacture of a multitude of parts, including valves, turbine components, welding rods, automotive injectors or surgical devices.
With more than 110 years of experience in steel manufacturing and continuous research in the field of metallurgy, the company guarantees optimal steel solutions for the demanding applications of its customers from the automotive, construction, process industry as well as the aerospace, nuclear and medical sectors.
Easy Machining
All this, by improving chip breakability and the surface finish of the parts.
With UGIMA® grades, this real achievement (performance level) is accessible to all types of machines and tools.
*with a constant tool lifetime – **after optimising cutting conditions
Technical support
Experts available throughout the world to help you. They can provide you with information and help you optimise your back-office or in-situ cutting conditions.
The UGIMA® solution and Ugitech’s technical support are unsurpassed!
Sustainable management of our heritage is an ethical and ecological necessity. It is also an economic imperative, which requires achieving the lowest possible life-cycle cost over the structure's service life.
In the most exposed parts of the structure, stainless steel reinforcing bars are the most efficient solution to ensure the durability of concrete. Stainless steel rebars are used for repairs and for new works, partially or completely replacing carbon steels, both in precast products and for the execution of cast-in-situ structures.
In addition to their excellent corrosion resistance which ensures a long service life for structures over several decades, the UGIGRIP® range provides a guarantee of:
Grades with high mechanical properties.
The UGI® grades offer all possible options in terms of grade, diameter, end finishing, and quantity. They are available ex-works or ex-stock.
Alloy welding wires.
UGICHROM® combines the high effi ciency of micro fissuring chromium plating with the technology of Ugitech's most advanced bars. For our customers, this guaranteed zero-defect solution is indispensable for many cutting edge applications (offshore, nuclear, wind power, aeronautics, etc.).
A wire that lasts, doesn’t stretch out of shape, and practically eliminates maintenance.
Breaking loads : UGIFIL® Over 135 kg/mm².
Elongation : UGIFIL® Less than 3 %.
A complete range of products used for concrete rebars. These stainless steel rebars are the solution to the problems encountered today in building and construction. They guarantee safety, durability, reduced maintenance costs andimproved living conditions. UGIGRIP®
Martensitic and ferritic grades characterized by their excellent levels of mechanical or magnetic properties.
Our range of improved machinability grades recognized by users. This process allows unparalleled cutting conditions and tool wear levels without affecting the intrinsic properties of the grades. We offer a growing range in a UGIMA® version.
The generation of UGIMA® that gives an additional boost to the productivity of grades 1.4305,1.4404, and 1.4307.
The optimum magnetism/machinability compromise in stainless steel.
An excellent compromise between corrosion resistance and the mechanical properties of the austeno-ferritic grades (Duplex).
Obtained with the ESR process, these stainless refractory products with improved cleanliness and structure respond to the strictest requirements of high-tech industries.
Our isoscele triangles mainly dedicated to Oil & Gas filtration.
The "must-have" for Slicklines in the Oil & Gas industry.
All Slick lines are 100 % Eddy Current tested before delivery to ensure that surfaces are free of cracks, and now an additional process has been added to detect defects under the surface, which is not normally possible with EC testing.
Ugitech can offer a wide range of grades, including Austenitic Stainless Steels, Duplex and Super Duplex grades and Nickel or Cobalt based alloys.
Stainless steel welding wires.
Hauptsitz
Ugine Cedex, France
Webseite
Umsatz
601-800M USD
Anzahl der Mitarbeiter
1000+
Gründungsjahr
1908
Art
Hersteller
Patente
Ugitech patents portfolio consists of 19 granted patents and 9 pending patents.
Qualitätszertifikate
ISO 9001; IATF 16949; EN 9100; EN 9120; ISO 13485; ISO 17025
Umwelt-Zertifizierungen
ISO 14001, ISO 50001
Certifications
ISO 9001
, IATF 16949
, EN 9100
, EN 9120
, ISO 13485
, ISO 17025
, ISO 14001
, ISO 50001
Sie haben eine E-Mail mit dem Link zum Zurücksetzen Ihres Passworts erhalten.
https://eservices.ugitech.com/
Automobil
Bau
Allgemeine Fahrzeugteile
Lebensmittelindustrie
Energie
Herstellung
Flüssigkeitssysteme
Mechanische Systeme
Elektronik
Chemie-Industrie
Luft- und Raumfahrt
Mineralöl- und Erdgasindustrie
Construction Materials
Konsumgüter
Ausrüstung für die Mineralöl- und Erdgasindustrie
Seefahrtbezogen
Healthcare
Fluidtechnische Anlagen
Materialien für Luft- und Raumfahrt
Elektronische Komponenten
Schiffsbau und Seefahrtstrukturen
Atomenergie
Dekorative Applikationen
Household Utensils
Medizinische Ausrüstung
Sensoren
Armaturen
Fahrzeugstruktur
Marine Shafts
Nuclear Plants
Schiffsarmaturen
Metallurgie
Bauelemente
Handgeführte Werkzeuge
Pneumatic Tools
Präzisionsmechanik
Ventile
Iron & Steel Products
Verbrennungsmotoren
Bearbeitung
Metallarmaturen
Rohrleitungen
Verteidigung
Wellen
Befestigungselemente für die Luft- und Raumfahrt
Schrauben
Haushaltselektrogeräte
Pumpen & Motoren
Rebar Steel
Landwirtschaft
Materials For Aerospace Construction
Motoren und Triebwerke für Luft- und Raumfahrt
Muttern
Papierindustrie
Pharmaindustrie
Uhren
Zahnräder
Zeitmessung
Federn
Waffen
Aerospace Fittings
Boiler & Wärmetauscher
Brenner & Boiler
Gas- und Dampfturbinen
Landwirtschaftliche Maschinen und Geräte
Verbindungselemente
Braking System
Building Structures
Container & Tanks
Drehschwingmechanismen
Flüssigkeitsspeicherung
Furnace Parts
Implantate
Industrieöfen
Kompressoren
Kupplungen
Luft- und Abgaskanäle
Militärtechnik
Schneiden
Schneidwerkzeuge
Shafts & Couplings
Spring Steels
Straßenfahrzeugsysteme
Besteck & Geschirr
Chirurgische Instrumente
Kochgeschirr
Küchenausstattung
Motorblock und -komponenten
Zahnmedizin
Zahnmedizinische Instrumente
Zahnärztliche Ausrüstung
Düsen
Gießformen
Messtechnik
Propeller
Schweißung
Sea Water Applications
Spanlose Arbeitsausrüstung
Sportausrüstung und -einrichtungen
Wassersportausrüstung
Grade | Shape | ||
---|---|---|---|
The UGI 4313 | Bar, Rod, Wire | JIS SUSF6NM, DIN 1.4313, ISO X3CrNiMo13-4, EN X3CrNiMo13-4, DIN X3CrNiMo13-4, ISO 4313-415-00-I, EN 1.4313, UNS S41500 | ISO 15510 |
UGI 202N-Grade 1 | Wire, Rod, Bar | JIS SUS202, DIN 1.4374, UNS S20200, AISI 202, EN 1.4374, DIN X8CrMnNiN18-9-5, EN X8CrMnNiN18-9-5 | EN 10088-3 |
UGI 209 | Bar, Wire, Rod | DIN 1.4455, UNS S20910, ASTM XM-19, EN X2CrNiMnMoN20-16, EN 1.4455, DIN X2CrNiMnMoN20-16 | NACE MR 0175 |
UGI 316Ti | Bar, Rod, Wire | DIN 1.4571, UNS S31635, AISI 316Ti, AFNOR Z6CNDT17-12, DIN X6CrNiMoTi17-12-2, EN X6CrNiMoTi17-12-2, EN 1.4571, JIS SUS316Ti, SS 2350, BS 320S31 | EN 10088-3, ASTM A240, ASTM A182, EN 10272 |
UGI 4029 | Bar, Wire, Rod | AISI 420F, EN X29CrS13, DIN X29CrS13, DIN 1.4029, EN 1.4029, EN 1.4020 | EN 10088-3 |
UGI 4057 AIR | Bar | AISI 431, EN 1.4057, DIN X15CrNi17-3, SS 2321, DIN 1.4057, BS S80, UNS S43100, DIN X17CrNi16-2, JIS SUS431, ASTM S43100, EN X17CrNi16-2, EN X15CrNi17-3, AFNOR Z15CN17-03, DIN 1.4044 | EN 10088-3, EN 3490, AFNOR 9160C |
UGI 4062 | Bar, Wire, Rod | UNS S32202, Alloy 2202, DIN 1.4062, EN 1.4062, AFNOR X2CrNiN22-2 | |
UGI 4105 | Bar, Billet | DIN 1.4105, EN X6CrMoS17, EN 1.4105, DIN X6CrMoS17, AISI 430F | EN 10088-3, ASTM A582, ASTM F899 |
UGI 4114 | Bar, Wire, Rod, Billet | EN X6CrMo19-2, EN 1.4114, UNS S18200, DIN X6CrMo19-2, ASTM XM-34, DIN 1.4114 | ASTM A582 |
UGI 4116N | Bar, Rod, Wire | EN 1.4116, DIN X50CrMoV15, DIN 1.4116, AFNOR 1.4116, EN X50CrMoV15 | EN 10088-3, NFA-36-711, SEW 400 |