Universal Stainless, headquartered in Bridgeville, PA, produces semi-finished and finished specialty steel long products and plate including stainless steel, tool steel, bearing steel, gear steel and aircraft quality low alloy steels. These can be manufactured into a wide variety of grades and product forms.
Hauptsitz
Bridgeville,Pennsylvania, United States
Webseite
Art
Hersteller und Verarbeiter
Certifications
AS 9100
, ISO 9001
, IEC 17025
, ISO 17025
, ISO 45001
Grade | Shape | ||
---|---|---|---|
13-8 PH | Bar | 13-8 PH, EN 13Cr-8Ni, UNS S13800, DIN 1.4534, AISI 632, ASTM XM-13 | AMS 5629, AMS 5864, ASTM A564, ASME SA564, ASTM A705, ASTM F899, HMS 6-1105, AMS STD-2154 |
15-5 PH | Bar, Plate | 15-5 PH, ASTM XM-12, UNS S15500, DIN X4CrNiCuNb16-4, EN X5CrNiCu15-5, DIN 1.4540, DIN 1.4545 | AMS 5659, AMS 5862, ASTM A564, ASTM A705, ASME SA564, Boeing BMS 7-240, Boeing BMS 7-351, SPPCA-EN-SOW-0036, Liebher LAT 1-9037, AMS STD-2154 |
17-4 PH | Bar, Plate | 17-4 PH, AISI 630, UNS S17400, DIN 1.4542, EN X5CrNiCuNb16-4 | AMS 5643, AMS 5604, AMS 5622, ASTM A564, ASTM A705, ASME SA564, MSRR 6601, AMS STD-2154 |
17-7 PH | Bar, Plate | 17-7 PH, AISI 631 | AMS 5644, ASTM A564 |
AISI 302 | Bar, Plate | AISI 302 | |
AISI 303 | Bar, Plate | AISI 303 | |
AISI 303Se | Bar | AISI 303Se, UNS S30323 | AMS 5640, AMS 5641, ASTM A320, ASTM A582, FED QQ-S-763, FED QQ-S-764, MIL-S-7720 |
AISI 304L | Bar, Plate | AISI 304L, UNS S30403, DIN 1.4307, EN X2CrNi19-1-1 | AMS 5647, AMS QQ-S-763, ASTM A276, ASTM A479, MB 0160-034, MB 0160-037 |
AISI 309 | Plate | AISI 309 | |
AISI 309S | Plate | AISI 309S | |