The plant focuses on producing value-added steel, with 214,000 tonnes produced in August 2010, out of 252,000 tonnes total of saleable steel produced.
Hauptsitz
Visakhapatnam,Andhra Pradesh, India
Webseite
Art
Hersteller und Händler
Certifications
ISO 9001
, OHSAS 18001
, ISO 14001
Grade | Shape | ||
---|---|---|---|
IS 20C15 | Bar | IS 20C15 | IS 2062 |
IS 27C15 | Bar | IS 27C15 | IS 2062 |
IS Fe415 | Bar | IS Fe415 | IS 1786 |
IS Fe500 | Bar | IS Fe500 | IS 1786 |
IS Fe500D | Bar | IS Fe500D | IS 1786 |
IS Fe550 | Bar | IS Fe550 | IS 1786 |
SAE 1008 | Wire, Rod | SAE 1008 | ASTM A510 |
SAE 1010 | Wire, Rod | SAE 1010 | ASTM A510 |
SAE 1012 | Wire, Rod | SAE 1012 | ASTM A510 |
SAE 1015 | Wire, Rod | SAE 1015 | ASTM A510 |