Villares Metals offers complete solutions for various segments and industries. Its portfolio includes: high-speed steels, tool steels (hot work, cold work and plastic molds), stainless steel, valve steels, special alloys and forgings.
Hauptsitz
Rotterdam, Netherlands
Art
Hersteller und Verarbeiter
Certifications
OHSAS 18001
, ISO 14001
, AD 2000
, ISO 9001
, ISO 16949
, IEC 17025
, ISO 17025
Grade | Shape | ||
---|---|---|---|
ASTM F51 | Tube | ASTM F51, UNS S31803, EN 1.4462 | |
ASTM F53 | Tube | ASTM F53, UNS S32750, Alloy 2507, EN 1.4410 | |
ASTM F55 | Tube | ASTM F55, UNS S32760, EN 1.4501 | |
ASTM F60 | Tube | ASTM F60, UNS S32205, Alloy 2205, EN 1.4462 | |
ASTM F61 | Tube | ASTM F61, UNS S32550, EN 1.4507 | |
ASTM XM-12 | Tube | ASTM XM-12, 15-5 PH, UNS S15500, DIN 1.4540 | |
ASTM XM-13 | Tube | ASTM XM-13, 13-8 PH, UNS S13800, DIN 1.4534 | |
SAE 630 | Tube | SAE 630, 17-4 PH, DIN 1.4542, EN 1.4548, UNS S17400 | |
SAE 631 | Tube | SAE 631, 17-7 PH, DIN 1.4568 | |
SAE 660 | Tube | SAE 660, EN 1.4980 | |