Aluminum and Metal Services Corp. (ALMETCO) is a native Puerto Rico enterprise founded in 1955. We specialize in the processing and distribution of aluminum and stainless steel materials. ALMETCO serves the industrial, commercial, and retail markets, as well as the general consumer.
Hauptsitz
San Juan, Puerto Rico
Webseite
Art
Processor and Distributor
Grade | Shape | ||
---|---|---|---|
AA 1100 | Sheet | AA 1100 | |
AA 2024 | Sheet | AA 2024 | |
AA 3003 | Bar, Sheet | AA 3003 | |
AA 5005 | Bar, Sheet | AA 5005 | |
AA 5052 | Bar, Sheet | AA 5052 | |
AA 6061 | Plate | AA 6061 | |
AA 6063 | Angle, Bar, Channel | AA 6063 | |
AA 7075 | Sheet | AA 7075 | |
AISI 304 | Tube, Bar, Profile, Rod, Angle, Pipe, Sheet, Plate | AISI 304 | |
EN AW-3105 | Bar, Sheet | EN AW-3105 | |