Wo Lee Steel Company Limited has become a reputable supplier of a wide range of steel materials and products for the manufacturing and construction industries both in Hong Kong and overseas. Wo Lee has diversified to extend its services to include Product Innovation and Processing Center to keep pace with the needs of an ever more demanding market worldwide.
Hauptsitz
Kowloon, Hong Kong SAR China
Webseite
Art
Hersteller und Verarbeiter
Grade | Shape | ||
---|---|---|---|
EN S260NC | Plate, Strip | EN S260NC | EN 10149-3 |
EN S275J0 | Plate, Strip | EN S275J0 | EN 10025-2 |
EN S275J0H | Plate, Strip | EN S275J0H | EN 10210-1, EN 10219-1 |
EN S275J2 | Plate, Strip | EN S275J2 | EN 10025-2 |
EN S275J2H | Plate, Strip | EN S275J2H | EN 10210-1, EN 10219-1 |
EN S275JR | Plate, Strip | EN S275JR | EN 10025-2 |
EN S275M | Plate, Strip | EN S275M | EN 10025-4 |
EN S275ML | Plate, Strip | EN S275ML | EN 10025-4 |
EN S275N | Plate, Strip | EN S275N | EN 10025-3 |
EN S275NL | Plate, Strip | EN S275NL | EN 10025-3 |