Steel Alloys & Services (SAS) strives to offer high-quality steel products and services for the oil and gas industry. We are dedicated to being the best possible supplier by providing on-time order processing and excellent customer service.
Hauptsitz
Houston,Texas, United States
Webseite
Art
Vertreiber
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
AISI 1008 | Bar | AISI 1008 | |
AISI 1095 | Bar | AISI 1095 | |
AISI 4130 | Bar | AISI 4130 | SAE 4130 |
AISI 4140 | Bar | AISI 4140 | |
Alloy 718 | Bar | Alloy 718 | |
Alloy 825 | Bar | Alloy 825, Incoloy 825 | |
Alloy 925 | Bar | Alloy 925 | |
ASTM 4140 | Bar | ASTM 4140 | |
UNS S41425 | Bar | UNS S41425, UNS S41427 | |